Thermoelectric properties of polycrystalline palladium sulfide

Liu-Cheng Chen, Bin-Bin Jiang, Hao Yu, Hong-Jie Pang, Lei Su, Xun Shi, Li-Dong Chen, Xiao-Jia Chen

文献索引:10.1039/C8RA01613E

全文:HTML全文

摘要

10.1039/C8RA01613E图片

Measurement of the electrical, thermal, and structural properties of palladium sulfide (PdS) has been conducted in order to investigate its thermoelectric performance. A tetragonal structure with the space group P42/m for PdS was determined from X-ray diffraction measurement. The obtained power factor of 27 μW cm−1 K−2 at 800 K is the largest value obtained for the transition metal sulfides studied so far. The maximum value of the dimensionless figure of merit is 0.33 at 800 K. These results indicate that binary bulk PdS has promising potential for good thermoelectric performance.