The dimensional changes of relined denture bases were evaluated in a laboratory study. Heat-cured resin, two autopolymerizing resins, microwave-activated resin and a new visible light-cured resin were used as relining materials in this study. The gaps between the metal die and the relined denture bases were measured immediately after the relining procedure and subsequently on the first day, first week, fourth week, and eight week. The relined denture bases were stored in distilled water at 37 degrees C between measurements. It was shown that dimensional changes in relined denture bases were influenced by the relining materials and procedures, and that heat-cured resin proved to have the smallest dimensional change as well as the greatest dimensional stability in comparison with the other relining materials and procedures.

相关化合物

结构式 名称/CAS号 全部文献
甲基丙烯酸甲酯交联聚合物 结构式 甲基丙烯酸甲酯交联聚合物
CAS:25777-71-3