Abstract

Spatial and temporal control is a key advantage for placement and rapid setting of light-activated resin composites. Conventionally, placement of multiple thin layers (<2 mm) reduces the effect of light attenuation through highly filled and pigmented materials to increase polymerisation at the base of the restoration. However, and although light curing greater than 2 mm thick layers is not an entirely new phenomenon, the desire amongst dental practitioners for even more rapid processing in deep cavities has led to the growing acceptance of so-called “bulk fill” (4–6 mm thick) resin composites that are irradiated for 10–20 s in daily clinical practice. The change in light transmission and attenuation during photopolymerisation are complex and related to path length, absorption properties of the photoinitiator and pigment, optical properties of the resin and filler and filler morphology. Understanding how light is transmitted through depth is therefore critical for ensuring optimal material properties at the base of thick increments. This article will briefly highlight the advent of current commercial materials that rationalise bulk filling techniques in dentistry, the relationship between light transmission and polymerisation and how optimal curing depths might be achieved.

Latest Articles:

Thermo-setting glass ionomer cements promote variable biological responses of human dental pulp stem cells

2018-04-09

[10.1016/j.dental.2018.03.015]

Wear measurement of dental tissues and materials in clinical studies: A systematic review

2018-04-04

[10.1016/j.dental.2018.03.002]

Influence of Class V preparation on in vivo temperature rise in anesthetized human pulp during exposure to a Polywave® LED light curing unit

2018-03-29

[10.1016/j.dental.2018.03.003]

Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications

2018-03-26

[10.1016/j.dental.2018.03.006]

Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: Effect of ceramic thickness

2018-03-24

[10.1016/j.dental.2018.03.004]

More Articles...