Macromolecular Rapid Communications 2010-07-01

Design and Synthesis of Fast-Degrading Poly(anhydride-esters).

AshleyL Carbone, KathrynE Uhrich

Index: Macromol. Rapid Commun. 30(12) , 1021, (2009)

Full Text: HTML

Abstract

Fast-degrading, salicylate-based poly(anhydride-esters) were designed to degrade and release the active component, salicylic acid (SA), within 1 week. The polymer degradation was enhanced by using shorter or oxygen-containing aliphatic chains. A copolymer of diglycolic acid was also made with a salicylate-based diacid for comparison of polymer properties, including SA release. Both methods resulted in polyanhydrides with molecular weights ranging from 14 500 to 27 800 Da and displayed glass transition temperatures near physiological conditions, namely 33-40 degrees C. the homo- and copolymers completely degraded within one week releasing the chemically incorporated SA.


Related Compounds

  • 2,2'-oxydiacetyl c...

Related Articles:

Antitrypanosomal activities and cytotoxicity of some novel imido-substituted 1,4-naphthoquinone derivatives.

2012-01-01

[Arch. Pharm. Res. 35(1) , 27-33, (2012)]

Design, synthesis and evaluation of diazadibenzocrown ethers as Pb(2+) extractants and carriers in plasticized cellulose triacetate membranes.

2001-07-06

[Talanta 54(6) , 1195-204, (2001)]

Synthesis and CO2 Solubility Studies of Poly (ether carbonate) s and Poly (ether ester) s Produced by Step Growth Polymerization. Tan B, et al.

[Macromolecules 38(5) , 1691-98, (2005)]

Preparation of chiral diphenyl substituted polyether-diester compounds. Bradshaw JS, et al.

[J. Org. Chem. 47(7) , 1229-1232., (1982)]

Small molecule antagonists of cell-surface heparan sulfate and heparin-protein interactions. Weiss RJ, et al.

[Chem. Sci. 6(10) , 5984-5993, (2015)]

More Articles...