Effect of maleic acid and ethylenediaminetetraacetic acid on the shear bond strength of RealSeal SE sealer to root canal dentin.
N V Ballal, A Tweeny, J C Baumgartner, K Ginjupalli, V Saraswathin
文献索引:Eur. J. Prosthodont. Restor. Dent. 21(4) , 152-6, (2013)
全文:HTML全文
摘要
Aim of this study was to evaluate the effect of 7% maleic acid and 17% ethylenediaminetetraacetic acid (EDTA) on the shear bond strength of RealSeal SE sealer to root canal dentin. Twenty incisors were split into coronal, middle and apical third and were treated in the following manner: Group 1: 5 ml of saline (1 minute). Group 2: 2.5% sodium hypochlorite (5 ml/min) followed by 79% maleic acid (5 ml/min). Group 3: 2.5% sodium hypochlorite (5 ml/min) followed by 17% EDTA (5 ml/min). Sealer was the placed on the root dentin and samples were subjected to bond strength measurement. There was no significant difference in bond strength between maleic acid and 17% EDTA in coronal & middle third. However, in apical third, 7% maleic acid showed higher bond strength. Least bond strength was observed with saline. Bond strength was maximum in apical third for both 7% maleic acid and 17% EDTA.
相关化合物
相关文献:
2014-12-01
[Food Chem. Toxicol. 74 , 131-8, (2014)]
2013-06-21
[Life Sci. 92(23) , 1110-7, (2013)]
2014-01-01
[Environ. Technol. 35(9-12) , 1165-74, (2014)]
2013-01-01
[Water Sci. Technol. 67(11) , 2488-93, (2013)]
2015-12-01
[J. Biomed. Mater. Res. A 103 , 3843-51, (2015)]