Design and Synthesis of Fast-Degrading Poly(anhydride-esters).
AshleyL Carbone, KathrynE Uhrich
文献索引:Macromol. Rapid Commun. 30(12) , 1021, (2009)
全文:HTML全文
摘要
Fast-degrading, salicylate-based poly(anhydride-esters) were designed to degrade and release the active component, salicylic acid (SA), within 1 week. The polymer degradation was enhanced by using shorter or oxygen-containing aliphatic chains. A copolymer of diglycolic acid was also made with a salicylate-based diacid for comparison of polymer properties, including SA release. Both methods resulted in polyanhydrides with molecular weights ranging from 14 500 to 27 800 Da and displayed glass transition temperatures near physiological conditions, namely 33-40 degrees C. the homo- and copolymers completely degraded within one week releasing the chemically incorporated SA.
相关化合物
相关文献:
2012-01-01
[Arch. Pharm. Res. 35(1) , 27-33, (2012)]
2001-07-06
[Talanta 54(6) , 1195-204, (2001)]
Synthesis and CO2 Solubility Studies of Poly (ether carbonate) s and Poly (ether ester) s Produced by Step Growth Polymerization. Tan B, et al.
[Macromolecules 38(5) , 1691-98, (2005)]
Preparation of chiral diphenyl substituted polyether-diester compounds. Bradshaw JS, et al.
[J. Org. Chem. 47(7) , 1229-1232., (1982)]
Small molecule antagonists of cell-surface heparan sulfate and heparin-protein interactions. Weiss RJ, et al.
[Chem. Sci. 6(10) , 5984-5993, (2015)]