| Name | gold atom |
|---|---|
| Synonyms |
Gold Thinfoil, 0.006mm (0.00024 in.) thick, not certified pinhole free
GOLD SPLATTER Gold nanopticles, cboxy-functionalized, 3kDa PEGylated, OD: 50, 540nm absorption AURIC GOLD ULTRATHIN Gold wire, 1.4mm (0.055 in.) dia Gold nanopticles, supplied in 0.1mM PBS, reactant-free OD1, 526nm absorption Gold nanopticles, supplied in 0.1mg/mL sodium citrate with stabilizer, OD: 1, 572nm absorption Gold nanopticles, biotin to functionalized, PEGylated, OD: 50, supplied in purified water, 515 to 520nm absorption Gold nanopticles, amine-functionalized, 3kDa PEGylated, OD: 50, 572nm absorption GOLD ISTANDD Gold nanopticles, amine-functionalized, 3kDa PEGylated, OD: 50, 553nm absorption GOLD STANDD SOLUTION Gold Palladium wire, 0.2mm (0.008 in.) dia., Annealed, Temper: softest 0.g/ft Gold foil, 0.25mm (0.01 in.) thick Gold wire, 0.813mm (0.032 in.) dia Gold wire, 0.2mm dia., trace GOLD PALLADIUM BRIGHT BRUSHING GOLD Gold nanopticles, supplied in 0.1mM PBS OD: 1, 548nm absorption GOLD SINGLE ELEMENT PLASMA STANDD Gold nanopticles, cboxy to functionalized, 3kDa PEGylated, OD: 50, 515 to 520nm absorption Gold nanopticles, amine-functionalized, 3kDa PEGylated, OD: 50, 530nm absorption Gold nanopticles, supplied in 0.1mM PBS, reactant-free OD1, 520nm absorption E 175 GOLD SPONGE Gold plasma standd solution, Au 1000μg/mL GOLD PLASMA EMISSION SPECTROSCOPY STANDD Gold nanorods, 9 to 15nm dia. x 46 to 56nm length, dispersion in water, 800nm Absorption, negatively chged AURUM STANDD SOLUTION Glod Gold nanorods, 9 to 15nm dia. x 55 to 65nm length, dispersion in water, 850nm Absorption, positively chged Gold wire, 1.0mm (0.04 in.) dia GOLD PHOSPHORUS Gold nanopticles, supplied in 0.1mg/mL sodium citrate with stabilizer Gold nanopticles, supplied in 0.1mg/mL sodium citrate with stabilizer, OD: 1, 548nm absorption GOLD, PLASMA STANDD SOLUTION Gold nanopticles, supplied in 0.1mM PBS OD: 1, 553 nm absorption Gold nanopticles, biotin-functionalized, PEGylated, OD: 50, supplied in purified water, 530nm absorption Gold wire, 0.0127mm (0.0005 in.) dia., 4.88m (16 ft.) GOLD PLATING SOLUTION GOLD SOL Gold slug, 3.175mm (0.125 in.) dia. x 3.175mm (0.125 in.) length GOLD METAL Gold nanopticles, cboxy-functionalized, 3kDa PEGylated, OD: 50, 520nm absorption Au MFCD00003436 Gold wire, 2.0mm (0.08 in.) dia Gold standd solution, 1 mg/ml Au in 0.5N HCl GOLD PLASMA EMISSION STANDD gold-197 Gold nanopticles, biotin-functionalized, PEGylated, OD: 50, supplied in purified water, 540nm absorption GOLD STANDD GOLD SINGLE ELEMENT STANDD Gold nanopticles, amine-functionalized, 3kDa PEGylated, OD: 50, 564nm absorption AUROUS Gold nanopticles, amine-functionalized, 3kDa PEGylated, 0D50, 520nm absorption Gold nanopticles, supplied in 0.1mM PBS OD: 1, 530 nm absorption GOLD I/DSTANDD EINECS 231-165-9 Gold nanopticles, supplied in 0.1mM PBS OD: 1, 526nm absorption Gold nanopticles, biotin-functionalized, PEGylated, OD: 50, supplied in purified water, 553nm absorption GOLD POWDER Gold nanopticles, cboxy-functionalized, 3kDa PEGylated, OD: 50, 564nm absorption |
| Density | 19.3 g/mL at 25 °C(lit.) |
|---|---|
| Boiling Point | 2808 °C(lit.) |
| Melting Point | 1063 °C(lit.) |
| Molecular Formula | Au |
| Molecular Weight | 196.967 |
| Flash Point | 4 °C |
| Exact Mass | 196.966507 |
| Index of Refraction | n20/589.3 1.523 |
| Storage condition | 2-8°C |
| Stability | Stable. May react with halogens, strong oxidizing agents, ammonia, hydrogen peroxide. Reaction with ammonia or hydrogen peroxide may form explosive materials. |
| Water Solubility | H2O: soluble |
CHEMICAL IDENTIFICATION
HEALTH HAZARD DATAACUTE TOXICITY DATA
|
| Personal Protective Equipment | Eyeshields;Gloves;type N95 (US);type P1 (EN143) respirator filter |
|---|---|
| Hazard Codes | Xi,Xn,F |
| Risk Phrases | R36/38 |
| Safety Phrases | S26-S36/37/39-S45-S62-S36/37 |
| RIDADR | UN 1789 8/PG 3 |
| WGK Germany | 3 |
| RTECS | MD5420000 |
| Packaging Group | II |
| Hazard Class | 6.1 |